- Joined
- May 9, 2020
- Messages
- 71
- Reaction score
- 21
So just got a cerium oxide scratch removal kit and practiced on a little old 20gal for about 2hrs and ended up way worse than I started lol..I do construction for a living and have even done a lot of glass work but being tempered it’s just all new to me. I ended up with a cloudy scratchy area that I was doing that literally only had a few little straight scratches. It now looks like I took a metal bristle brush and swirled it in circles which is pretty much what I felt like I did but with the oxide. I tried going through the pads and ended with the fluffy ones but still didn’t touch it...any advice? Did I start with too coarse of paper? Maybe too long? I’ll post a few pics of what I got.