Troylee
all about the diy!!!!!
View Badges
Ultimate Member
Reef Squad
Excellence Award
R2R App User
Moderator Emeritus
Hospitality Award
ThreadAward
My Tank Thread
My Aquarium Showcase
Weldon 40 two part consist of a part "a" acrylic monomer and part "b" a hardner.... It's very similiar tocan you explain the weldon 40 2-part?
Fiberglass resin and hardner if you ever worked with that.... It makes a super big mess but it gets the job done lol...
Pretty much since the regular hobbiest dont have a big oven to anneal it and get it to it's maximum strength I
Don't really recommend it.... Using 40 out of the bottle is no stronger than any solvent like 3 or 4 and a lot tougher to use... It for sure has it place but for you guys I would stick with solvents honestly it's more forgiving and way faster..;)